Effect of silanized silica nanofiller on tack and green strength of selected filled rubbers

The full text article is not available for purchase.

The publisher only permits individual articles to be downloaded by subscribers.

BACKGROUND: Tack and green strength of filled and gum (unfilled) natural rubber (NR), poly(styrene‐co‐butadiene) rubber (SBR), polybutadiene rubber (BR) and (SBR‐BR) blend with different loadings of reinforcement agent, silanized silica nanofiller (Coupsil 8113), were studied and the results compared and discussed.

RESULTS: It was found that silica was fully dispersed in rubber matrix after 13 min of mixing. In addition, with some exceptions for NR and (SBR‐BR) blend, filler loading decreased the tack strength of the studied filled rubbers. Green strength and Mooney viscosity increased with filler loading for all studied filled rubbers but with different rates and amounts. The optimum filler loadings for NR and (SBR‐BR) filled blend were 30 and 10 phr, respectively. Tacks of NR filled rubbers were much higher than those of synthetic filled rubbers.

CONCLUSION: It was concluded that filler loading alters substantially the tack and green strength of the rubbers under investigation. Copyright © 2009 Society of Chemical Industry
No References
No Citations
No Supplementary Data
No Article Media
No Metrics

Keywords: green strength; rubber; silanized silica nanofiller; tack

Document Type: Research Article

Publication date: April 1, 2009

More about this publication?
  • Access Key
  • Free content
  • Partial Free content
  • New content
  • Open access content
  • Partial Open access content
  • Subscribed content
  • Partial Subscribed content
  • Free trial content
Cookie Policy
X
Cookie Policy
Ingenta Connect website makes use of cookies so as to keep track of data that you have filled in. I am Happy with this Find out more