An attempt to recover strength of oxidized SiC/SiC composite by means of a deoxidation treatment
Authors: Morishita, K.; Ochiai, S.; Okuda, H.; Nakayama, H.; Sato, M.
Source: Composite Interfaces, Volume 12, Numbers 8-9, 2005 , pp. 853-858(6)
Publisher: VSP, an imprint of Brill
Abstract:
An attempt was made to recover the strength of a PIP-processed SiC/SiC composite exposed in air at high temperatures by means of the deoxidization treatment with CO gas. By deoxidation treatment at 1723 and 1823 K for the composite specimen oxidized at 1573 K, the strength of deoxidized specimens became higher by around 4 and 1.5 times than that of oxidized one, respectively.Keywords: SIC/SIC COMPOSITE; INTERFACE; OXIDATION; DEGRADATION; DEOXIDATION; STRENGTH
Document Type: Letter section
DOI: http://dx.doi.org/10.1163/156855405774984057
Publication date: 2005-10-01
- In this: publication
- By this: publisher
- In this Subject: Chemistry , Engineering/Technology , Materials & Manufacturing
- By this author: Morishita, K. ; Ochiai, S. ; Okuda, H. ; Nakayama, H. ; Sato, M.

Shopping cart
Receive new issue alert
Get Permissions