Column flotation of high grade fluorite without wash water addition

Authors: Aliaga, W.; Sampaio, C. H.; Brum, I. A. S.; Ferreira, K. R. S.; Batistella, M. A.

Source: Mineral Processing and Extractive Metallurgy, Volume 116, Number 4, 2007 , pp. 251-256(6)

Publisher: Maney Publishing

Buy & download fulltext article:

OR

Price: $48.00 plus tax (Refund Policy)

Abstract:

The present paper presents the results of fluorite flotation carried out on a column cell without wash water addition. Concentrate flow was obtained by making tailing flows smaller than feed flows. Hence, part of the feed water was carried up within bubble wakes. No pulp/froth interface was established. A high recovery was obtained in a 2 m collection zone column. The recovery reached >80% with a grade of ?90%. It was found that the recovery depended on the value of the difference between the feed flow and tailing flow. In addition, a straight line between the surface velocity of mineral and the recovery was found. It appears that a maximum capacity of solid is ?10 g min?1 cm?2.

Keywords: FLUORITE; COLUMN CELL; FLOTATION

Document Type: Research Article

DOI: http://dx.doi.org/10.1179/174328507X198654

Publication date: 2007-12-01

More about this publication?
Related content

Tools

Key

Free Content
Free content
New Content
New content
Open Access Content
Open access content
Subscribed Content
Subscribed content
Free Trial Content
Free trial content

Text size:

A | A | A | A
Share this item with others: These icons link to social bookmarking sites where readers can share and discover new web pages. print icon Print this page