Journal of Materials Science logo Springer logo

Publisher: Springer

Related content
Volume 32, Number 18, 1997

< previous issue | all issues | next issue >

Particle fracture in metal-matrix composite friction joints
pp. 4739-4748(10)
Authors: MALDONADO C.; NORTH T.H.

Fracture mechanisms of poly(ethylene terephthalate) and blends with styrene-butadiene-styrene elastomers
pp. 4749-4758(10)
Authors: TANRATTANAKUL V.; PERKINS W.G.; MASSEY F.L.; MOET A.; HILTNER A.; BAER E.

Strength and fracture toughness of in situ-toughened silicon carbide
pp. 4777-4782(6)
Authors: CHO D-H.; KIM Y-W.; KIM W.

Agglomeration parameter, aggregation number, and aggregate porosity
pp. 4803-4806(4)
Authors: SHIN H-S.; LEE B-K.

Carbide precipitation in some secondary hardened steels
pp. 4815-4820(6)
Authors: GINGELL A.D.B.; BHADESHIA H.K.D.H.; JONES D.G.; MAWELLA K.J.A.

The hot compaction of SPECTRA gel-spun polyethylene fibre
pp. 4821-4832(12)
Authors: YAN R.J.; HINE P.J.; WARD I.M.; OLLEY R.H.; BASSETT D.C.

Preparation and properties of barium aluminosilicate glass-ceramics
pp. 4833-4836(4)
Authors: ZHOU W.; ZHANG L.; YANG J.

Structural transformation of dip coated CdS thin films during annealing
pp. 4837-4840(4)
Authors: NARAYANAN K.L.; VIJAYAKUMAR K.P.; NAIR K.G.M.; THAMPI N.S.; KRISHAN K.

Massive transformation in an Fe–Cu alloy
pp. 4847-4855(9)
Authors: HWANG N.M.; YOON D.Y.

Mechanical alloying synthesis and structural characterization of ternary Ni-Al-Fe alloys
pp. 4857-4864(8)
Authors: LIU Z.G.; GUO J.T.; ZHOU L.Z.; HU Z.Q.; UMEMOTO M.

Silicon oxide thin films prepared by a photo-chemical vapour deposition technique
pp. 4895-4900(6)
Authors: JANA T.; GHOSH S.; RAY S.

Anodic film formation on high strength aluminium alloy FVS0812
pp. 4909-4916(8)
Authors: SYKES J.; THOMPSON G.E.; MAYO D.; SKELDON P.

Gamma prime (gammaprime) precipitating and ageing behaviours in two newly developed nickel-base superalloys
pp. 4917-4923(7)
Authors: KIM H.T.; CHUN S.S.; YAO X.X.; FANG Y.; CHOI J.

Enhancing densification of zirconia-containing ceramic-matrix composites by microwave processing
pp. 4925-4930(6)
Authors: FANG Y.; CHENG J.; ROY R.; ROY D.M.; AGRAWAL D.K.

Wettability of NiAl by a liquid Ni–Si–B alloy
pp. 4931-4940(10)
Authors: GALE W.F.; FERGUS J.W.; INGRAM W.M.; KOOPMAN M.

Micromechanical analysis of the finite element calculation of a diffusional transformation
pp. 4941-4955(15)
Authors: GANGHOFFER J.F.; DENIS S.; GAUTIER E.; SJOSTROM S.

Synthesis and growth mechanism of ThO2–W–Mo alloy nanocomposite powder
pp. 4957-4965(9)
Authors: DEVAUX X.; THOMY A.; GHANBAJA J.

Adhesion strength of silver thick-film conductors by solder-free test
pp. 4967-4971(5)
Authors: ENOKIDO Y.; YAMAGUCHI T.

Structural effects of interaction between lanthanum cuprate and cerium dioxide
pp. 4991-4997(7)
Authors: MUKOVOZOV I.E.; EZERETS A.M.; VISHNIAKOV A.V.; FORNI L.; OLIVA C.

Fabrication of high aspect ratio silicon micro-tips for field emission devices
pp. 4999-5003(5)
Authors: CHUNG I.J.; MURFETT D.B.; HARIZ A.; HASKARD M.R.

Interfacial morphologies between alumina and silver-copper-titanium alloy
pp. 5011-5015(5)
Authors: HAO H.; WANG Y.; JIN Z.; WANG X.

< previous issue | all issues | next issue >

Key

Free Content
Free content
New Content
New content
Open Access Content
Open access content
Subscribed Content
Subscribed content
Free Trial Content
Free trial content

Text size:

A | A | A | A
Share this item with others: These icons link to social bookmarking sites where readers can share and discover new web pages. print icon Print this page