Wear logo Elsevier logo

Publisher: Elsevier

Related content
Volume 225, Number 2, April 1999

< previous issue | all issues | next issue >

Surface characterization of metal-on-metal hip implants tested in a hip simulator
pp. 708-715(8)
Authors: Wang A.; Yue S.; Bobyn J.D.; Chan F.W.; Medley J.B.

Wear of shelf-aged UHMWPE acetabular liners
pp. 728-733(6)
Authors: Lee K.-Y.; Lee K.H.

Fundamental study for all-ceramic artificial hip joint
pp. 734-742(9)
Authors: Kusaka J.; Takashima K.; Yamane D.; Ikeuchi K.

Wear patterns from fatigue life testing of a prosthetic heart valve
pp. 743-748(6)
Authors: Grigioni M.; Daniele C.; D'Avenio G.; Calcagnini G.; Barbaro V.

Ni-P and Mo: an excellent fretting wear resistant combination
pp. 749-757(9)
Authors: Okado J.; Shima M.; McColl I.R.; Waterhouse R.B.; Hasegawa T.; Kasaya M.

Wear of titanium carbide reinforced metal matrix composites
pp. 758-769(12)
Authors: Dogan O.N.; Hawk J.A.; Tylczak J.H.; Wilson R.D.; Govier R.D.

Sliding wear of cadmium against alumina
pp. 770-776(7)
Authors: Singh R.A.; Biswas S.K.; Kailas S.V.

Friction measurement on Al-Cu-Fe quasicrystalline and B2-type materials
pp. 784-788(5)
Authors: Zhang L.M.; Zhang H.C.; Zhou Q.G.; Dong C.

Abrasive wear behaviour of conventional and nanocomposite HVOF-sprayed WC-Co coatings
pp. 789-798(10)
Authors: Stewart D.A.; Shipway P.H.; McCartney D.G.

Microstructure and tribological properties of sulphide coating produced by ion sulphuration
pp. 799-805(7)
Authors: Zhuang D.-M.; Liu Y.-R.; Liu J.-J.; Fang X.-D.; Guang M.-X.; Cui Y.

Tribological behaviour of plasma-sprayed chromium oxide coating
pp. 814-824(11)
Authors: Ahn H.-S.; Kwon O.-K.

Comparison of slurry and dry erosion behaviour of some HVOF thermal sprayed coatings
pp. 825-834(10)
Authors: Hawthorne H.M.; Arsenault B.; Immarigeon J.P.; Legoux J.G.; Parameswaran V.R.

Tribological properties of smooth diamond coatings for cutting tools
pp. 843-847(5)
Authors: Huu T.L.; Schmitt M.; Paulmier D.; Mamalis A.G.; Grabchenko A.

Tribochemical polishing of silicon carbide in oxidant solution
pp. 848-856(9)
Authors: Zhu Z.; Muratov V.; Fischer T.E.

Thermally induced wear of ceramics
pp. 857-861(5)
Authors: Metselaar H.S.C.; Winnubst A.J.A.; Schipper D.J.

Size effect for specific energy in grinding of silicon nitride
pp. 862-867(6)
Authors: Hwang T.W.; Evans C.J.; Malkin S.

Tribological behavior of alumina reinforced with unidirectionally oriented SiC whiskers
pp. 868-873(6)
Authors: Lim D.-S.; Park D.-S.; Han B.-D.; Kan T.-S.

Friction and wear of SiC fiber-reinforced borosilicate glass mated to steel
pp. 885-895(11)
Authors: Zum Gahr K.-H.; Voelker K.

Control of wear applied to compressors: trends in lubricant analysis
pp. 905-912(8)
Authors: Carnero M.C.; LaTorre E.; Alcazar M.A.; Conde J.

Failure analysis of hydro-generator thrust bearing
pp. 913-917(5)
Author: Iliev H.

Novel instrumentation for evaluating stone impact wear of automotive paint systems
pp. 936-948(13)
Authors: Ramamurthy A.C.; Buresh G.A.; Nagy M.; Howell M.

Wear mechanism in graphite-copper electrical sliding contact
pp. 949-953(5)
Authors: Senouci A.; Frene J.; Zaidi H.

Laboratory simulation to select oil seal and surface treatment
pp. 954-961(8)
Authors: Shuster M.; Seasons R.; Burke D.

Lubrication in fretting-a review
pp. 962-967(6)
Authors: Zhou Z.R.; Vincent L.

Inorganic fullerene-like material as additives to lubricants: structure-function relationship
pp. 975-982(8)
Authors: Rapoport L.; Feldman Y.; Homyonfer M.; Cohen H.; Sloan J.; Hutchison J.L.; Tenne R.

Effects of surface defects on rolling contact fatigue of 60/40 brass
pp. 983-994(12)
Authors: Gao N.; Dwyer-Joyce R.S.; Beynon J.H.

Some influence parameters on greases lubricated rolling contacts service life
pp. 1004-1010(7)
Authors: Farcas F.; Gafitanu M.D.

Lubrication mechanisms of a sliding contact by simultaneous action of electric current and magnetic field
pp. 1011-1016(6)
Authors: El Mansori M.; Paulmier D.; Ginsztler J.; Horvath M.

Effect of environmental embrittlement on wear resistance of alloys in corrosive wear
pp. 1025-1030(6)
Authors: Shizhuo L.; Xiaoxia J.; Hongyun B.; Shu L.

Laboratory abrasive wear tests: investigation of test methods and alloy correlation
pp. 1031-1042(12)
Authors: Hawk J.A.; Wilson R.D.; Tylczak J.H.; Dogan O.N.

The corrosive wear behavior of Cr-Mn-N series casting stainless steel
pp. 1043-1049(7)
Authors: Bi H.Y.; Jiang X.X.; Li S.Z.

A comparison of laboratory abrasion and field wear results
pp. 1059-1069(11)
Authors: Tylczak J.H.; Hawk J.A.; Wilson R.D.

New experimental technique for the study and analysis of solid particle erosion mechanisms
pp. 1070-1077(8)
Authors: Talia M.; Lankarani H.; Talia J.E.

The role of passive oxide films on the degradation of steel in tribocorrosion systems
pp. 1078-1087(10)
Authors: Mischler S.; Spiegel A.; Landolt D.

Hydroabrasive wear behaviour and damage mechanisms of different hard coatings
pp. 1088-1099(12)
Authors: Hoppel H.W.; Mughrabi H.; Sockel H.-G.; Schmidt S.; Vetter G.

On the wear behavior of surface clad layers under high temperature
pp. 1114-1122(9)
Authors: Aoh J.-N.; Jeng Y.-R.; Chu E.-L.; Wu L.-T.

Physical vapour deposition duplex coatings for aluminium extrusion dies
pp. 1123-1130(8)
Authors: Bjork T.; Westergard R.; Hogmark S.; Bergstrom J.; Hedenqvist P.

Time-dependent friction response of plasma-sprayed molybdenum
pp. 1131-1140(10)
Authors: Usmani S.; Sampath S.

Structure and tribological behaviour of carbon nitride films
pp. 1141-1147(7)
Authors: Wei J.; Hing P.; Mo Z.Q.

Friction-induced microstructural variations in steels subjected to low-energy elevated-temperature nitrogen ion implantation
pp. 1148-1158(11)
Authors: Byeli A.V.; Kukareko V.A.; Boyarenko I.V.; Kolesnikova A.A.

Development and use of ASTM standards for wear testing
pp. 1159-1170(12)
Authors: Blau P.J.; Budinski K.G.

Surface characterization of wear particles
pp. 1171-1185(15)
Authors: Stachowiak G.W.; Podsiadlo P.

Applications of a non-contacting Kelvin probe during sliding
pp. 1186-1204(19)
Authors: Kasai T.; Fu X.Y.; Rigney D.A.; Zharin A.L.

Influence of contact configuration in fretting fatigue testing
pp. 1205-1214(10)
Authors: Pape J.A.; Neu R.W.

Application of a specialized capacitance probe in bearing diagnosis
pp. 1215-1221(7)
Authors: Yang Y.; Kurfess T.; Liang S.; Danyluk S.

Novel experimental techniques for investigating time resolved high speed friction
pp. 1222-1237(16)
Authors: Rajagopalan S.; Irfan M.A.; Prakash V.

Wear particle classification in a fuzzy grey system
pp. 1238-1247(10)
Authors: Peng Z.; Kirk T.B.

Impeller wear impact-abrasive wear test
pp. 1248-1257(10)
Authors: Wilson R.D.; Hawk J.A.

Interactions in silicon nitride ceramics vs. steel contact under fretting conditions
pp. 1276-1283(8)
Authors: Novak S.; Drazic G.; Kalin M.; Vizintin J.

Tribological properties of nanoscale alumina-zirconia composites
pp. 1293-1302(10)
Authors: Kerkwijk B.; Winnubst A.J.A.; Verweij H.; Mulder E.J.; Metselaar H.S.C.; Schipper D.J.

Cyclic contact fatigue of silicon nitride
pp. 1303-1308(6)
Authors: Legin Eyzop B.; Karlsson S.

A better approach to wear-rate representation in non-conformal contacts
pp. 1309-1314(6)
Authors: Ravikiran A.; Lim S.C.

Tribological properties of SiC and C-fiber reinforced glass matrix composites
pp. 1315-1321(7)
Authors: Reinicke R.; Friedrich K.; Beier W.; Liebald R.

Wear of Al2O3-SiC-(Al,Si) melt oxidised ceramic composites
pp. 1322-1326(5)
Authors: Jayaram V.; Biswas S.K.

Reciprocating friction and wear behavior of a ceramic-matrix graphite composite for possible use in diesel engine valve guides
pp. 1338-1349(12)
Authors: Blau P.J.; Dumont B.; Braski D.N.; Jenkins T.; Zanoria E.S.; Long M.C.

< previous issue | all issues | next issue >

Key

Free Content
Free content
New Content
New content
Open Access Content
Open access content
Subscribed Content
Subscribed content
Free Trial Content
Free trial content

Text size:

A | A | A | A
Share this item with others: These icons link to social bookmarking sites where readers can share and discover new web pages. print icon Print this page